Optimization and Production Practice of Top Slag Modifier for  IF Steel DC06 with 260 t BOF-RH Flowsheet
Hu Wei, Xu Bin, Huang Jiaqi, Zhu Wenrui, Li Ji, Li Renchun , Liu Junshan , Cheng Rijin
Special Steel . 2021, (3): 27 -30 .