Test and Practice on Capping Process of 250 mm x 2 000 mm  Casting Tail Slab of Nb-V-Ti Microalloying Low Alloy Steel SG610E
Cao Lei, Ma Baozhen, Huang Weiqing, Han Lihao, Shi Yongliang
Special Steel . 2021, (3): 31 -34 .