Research on Technology of Feeding Rare-earth Wires in Liquid in Stainless Steel Slab Continue Casting Mould
Lang Weiyun , Zhai Jun, , Chen Yang, Li Xiaojun , Chang Guodong
Special Steel . 2020, (3): 35 -38 .