A Study on Non-Metallic Inclusion in DQ Deep-Drawing Low Carbon Steel Casting Slab Produced by CSP Process 
Fei Shangcai , Jiang Xiaoxia, Gou Ningnian , Xu Nan
Special Steel . 2020, (4): 37 -39 .