Analysis on Cause of Upwarping of 20 Cr Steel Crankshaft Forgings and Process Improvement
Li Shichao, Li Jinbo, Fan Quanbao, Li Ang , Xu Xueliang
Special Steel . 2020, (5): 19 -21 .