A Study on Superplasticity of Cold Rolling 0.10C5Mn2Al Steel at Strain Rate 10 ~2 /s
Liu Sihan, Wang Cunyu , Wang Chang, Xu Haifeng , Cao Wenquan
Special Steel . 2020, (5): 55 -59 .