Study on Degassing Behavior and Inclusion in "VIM + ESR" and "NVIM + ESR" Smelting Processes of GH3128 Alloy
Fu Jianhui , Liu Tingyao, Zhang Jian , Lai Yu
Special Steel . 2020, (6): 15 -19 .