ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Process Development and Production Practice of 303F  Free-cutting Stainless Steel Φ9.0 mm Rod
Tu Yuguo, Zhang Guofu , Ye Gang, Xue Weibing , Zhang Wei
Special Steel . 2020, (6): 20 -23 .