ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Optimization of Heat Treatment Process of High Strength-Toughness U20Mn2SiCrNiMo Bainite Steel Rail
Yang Weiyu , Zhang Fengming, He Jianzhong, Li Zhili , Liu Yanjun