Effect of Post-Weld Heat Treatment on -20℃ Impact Toughness of Heat Affected Coarse Grain Zone of Steel 07MnCrMoVR
Feng Lulu, Qiao Wenwei , Lu Xiuyu , Zhou Feng
Special Steel . 2020, (6): 68 -71 .