ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

High Carbon Stranded Steel SWRH82B Central Carbon  Segregation Control Practice
Wang Wenpei, Liu Liexi, Li Hai, Xu Lei, Fan Shiwei , Ding Li
Special Steel . 2019, (5): 24 -27 .