Cause Analysis on Cracking of ML08A1 Steel Rivets for Non-Standard Special-Shaped Fasteners and Process Improvement
Zhao Mantang, Tao Qunnan, Chen Yongfeng, Lu Jihuan
Special Steel . 2021, (3): 39 -41 .