Analysis on Formation of Transverse Corner Cracks of Slab of Peritectic Steel Q345D by Slab Quenching Test and Process Improvement
Yan Huicheng, Cheng Xudong, Gong Yankun, Zhang Kai , Ma Jingchao
Special Steel . 2019, (5): 64 -66 .