Effect of Finish Rolling and Spinning Temperature on Phase Structure of Iron Oxide Skin of SCM435 Wire Rod
Wang Ningtao , Li Shilin, , Ruan Shipeng, Wang Lijun,
Special Steel . 2019, (4): 4 -6 .