Production Practice of 0Crl3C Steel in 60 t AOD by Primary Reduction Slag without Adding Fluorite
Feng Wenfu, Ma Fuping, Ye Fanxin, Guo Jian, Guo Zhibin , Fan Jianying
Special Steel . 2019, (4): 28 -30 .