ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Study on Mechanical Descaling Property of Oxide  Scale of ER70S-6 Welding Wire Steel
Li Hao, Zhang Yayun, Guo Huiying, Wang Na , Zhang Yu
Special Steel . 2019, (4): 66 -70 .