ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Development of High Scrap Ratio in Steelmaking Process of 180 t Converter
Guan Ting, Wang Yao , Liu Fei , Zou Changdong , Wang Jianhua