Development and Corrosion Resistance of Nb-V Microalloyed Cu-Bearing High Strength Weathering Steel
Yao Jitan, Sun Li, An Huilong, Xin Ruishan, Pan Jin, Zhao Yanqing , Ren Shuai
Special Steel . 2019, (3): 59 -61 .