Analysis on Strip Fracture of High Strength IF Steel Containing Phosphorus During Straightening in Pickling & Rolling and Process Improvement
Li Junsheng , Xue Renjie , Ma E , Cao Xiaoen , Luo Xiang
Special Steel . 2019, (2): 53 -56 .