Study on Structure and Performance of Coarse Grained Heat Affected Zone( CGHAZ) of Machinery Steel 960QT
Liu Xuhui , Zhang Bo , Xiao Aida, Ou Ling, Hao Chunhui
Special Steel . 2019, (1): 63 -67 .