ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Simulation Study on Melting Behavior of Manganese Ore Pellets  Containing Carbon in Converter Quarternary Slag
Zhang Bo, Wang Yufei, Wang Daping, Liu Lang , Hao Chunhui
Special Steel . 2018, (6): 16 -21 .