Effect of Electromagnetic Stirring on Solidification Structure of 1 t Electroslag Remelting Ingot of Alloy GH4169
Lü Da, Zhang Yunfei, Zhang Fuli, Han Yanguang, Ren Shuai, Cui Yi , Bai Lijuan
Special Steel . 2018, (5): 44 -47 .