Practice of Rolling Process for Φ 158.75 mm x25.4 mm Heavy Wall Tube of Martensite Stainless Steel 420M
Peng Jun, Wan Wuxia, Li Fuhua , Tang Ke
Special Steel . 2018, (4): 35 -37 .