Thermoplasticity of Continuous Casting Slab of High Strength Steel CR1030/1300MS for Auto
Cao Xiaoen, Cheng Di, Wu Zhijie, Jiang Limei , Zhang Kecai
Special Steel . 2018, (3): 1 -4 .