Thermodynamic Analysis on Calcium Sulphide Inclusions in Bearing Sulphur-Aluminium Steel GS35C-A and Process Improvement
Ji Dandan, Ye Fanxin, Zhang Jinhong, Dai Yonggang , Li Fuwei
Special Steel . 2018, (3): 5 -8 .