Production Practice for Low Carbon Steel QD08 Steelmaking by Natural Decarburization during 120 t RH Refining Process
Li Hai, Liu Liexi, Zhang Hongbiao, Jie Ruihua, Wang Liqing, Lu Man , Xu Lei
Special Steel . 2018, (3): 13 -16 .