Process Practice of Titanium Stabilizing Austenite Stainless Steel 321 Produced by EAF-AOD-LF-Slab Casting
Tan Jianxing, Wu Peng, Liu Ruizhi , Liu Mingsheng
Special Steel . 2018, (3): 28 -30 .