Effect of 210 t RH Refining Parameters on Cleanliness of Steelmaking-Rolling IF Steel and Process Optimization
Deng Birong, Zhang Bo, Zhou Jianfeng, Liu Lang , Li Chunxiao
Special Steel . 2018, (3): 31 -34 .