Effect of Controlled Rolling and Cooling Process on Structure and Mechanical Properties of Mushroom Cold Upsetting Steel
Hu Zhiyuan, Wei Zhanshan, Li Zhuang, Yu Tao , Li Zhaohua
Special Steel . 2018, (3): 62 -65 .