Research on Diffusion Behavior of Cr and Ni at Interface of Vacuum Hot-Rolled Q345B Carbon Steel-304 Stainless Steel Clad Plate
Wang Guanglei, Dang Jun , Zhai dongyü , Wang Changmin
Special Steel . 2022, (2): 27 -30 .