Effect of Residual Boron on Jominy Hardenability of 20CrMnTiH Steel and Process Control
Wang Zhilin, He Guoning, Gao Jianpeng, Jia Yu , Zhao Haidong
Special Steel . 2022, (2): 40 -43 .