Analysis and Control of Intermediate Cracks in Q235B Steel Continuous Casting Slab Produced by LD-Ladle Argon Blowing Route
Huang Hua, Shi Penzhao , Xu Lijun, Xia Chunxiang , Zhao Yingjie
Special Steel . 2022, (2): 55 -58 .