Study on Behavior of Inclusions Removal from GCr15  Bearing Steel by Refining Slag
Zhao Xinkai, Shi Yongsheng, Liu Shiyi, Wang Delong, Zhang Jiongming
Special Steel . 2022, (3): 14 -20 .