Mechanism Analysis and Process Improvement of YG1900 Ultra-High-Strength Steel's Non-Uniform Properties
DONG Xiaoliang , ZHANG Xiuli, XU Guangpeng , ZHENG Zhenyu, CAO Guang, LIAO Kai
Special Steel . 2022, (3): 52 -55 .