Effect of Tempering Temperature on Microstructure and Mechanical Properties of 20SiMnMo High Strength Steel
LIN Wenzheng, TIAN Rongbin, JIA Li, DUAN Baoyu , GAO Zhanyong
Special Steel . 2022, (3): 74 -78 .