Thermoplasticity of ESR Ingot of High Nitrogen Austenite Stainless Steel 0.05C-14Mn-19Cr-0.7N
Li Jianxin, Zhao Yingli, Zhang Yunfei, Ji Shuang, Zhang Kun , Xing Chengliang
Special Steel . 2018, (2): 6 -9 .