Process Practice on Improving Metallurgical Quality of Gear Steel 20CrMnTiH
Du Dongfii, Zhao Xiqing, Zhang Jianyuan, Tian Jinglin, Jia Wenjun
Special Steel . 2018, (2): 34 -37 .