ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Influence of Shot Peening Process on Performance of High Speed Steel M42-Spring Steel D6A Bi-Metal Band-Saw Blade
Li Dongliang, Kuang Xuguang , Deng Qunzhou, Li Jian
Special Steel . 2018, (1): 57 -60 .