ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

High Temperature Mechanical Properties of 280mm x 325mm Casting Bloom of Alloy Steel SAE8640
Wang Ningtao , Ruan Shipeng , Duan Luzhao , Wang Lijun
Special Steel . 2018, (1): 68 -70 .