ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Heat Treatment on Structure, Hardness and Aging Kinetics of Plastic Die Steel NAK80
Sun Guodong, Liu Changhua, Song Yongbin, Yang Xianqi
Special Steel . 2018, (2): 60 -64 .