Commercial Pilot Production on Replacing Partial Lime in Slag by Limestone in 60t Converter Steelmaking at Tangsteel
Li Chenxiao, Hao Huaqiang, Wang Shuhuan, Zhao Dingguo, Chen jianjun, Liu Shanxi
Special Steel . 2017, (6): 16 -18 .