Effect of Cooling Time from 800℃ to 500℃ on Phase Transition Behavior and Microstructure of Low Temperature Steel 9Ni
Yang Xiuzhi , Hua Wenlin , Yang Chunjie , Dong Chunfa
Special Steel . 2017, (5): 10 -12 .