Production Practice of Φ219.1mm x9.5mm Anti-Hydrogen Sulfide Corrosion Seamless Pipe Line Steel Tube X52QS
Wang Xuemin , Deng Xuyan , Li Jianqiang , Feng Ying , Li Yinzhen , Hu Chujiang
Special Steel . 2017, (5): 13 -16 .