Effect of Aging Temperature on Mechanical Properties and Structure of Secondary-Hardening Ultra-High Strength Steel M54
Wang Fei, Yang Zhuoyue, Pang Xuedong, Sun Yong , Zhai Yujia, Li Jianxin , Zhao Chengzhi , Wang Rui, Yan Xiaohong
Special Steel . 2017, (6): 67 -70 .