Effect of 100 t LF Refining Slag Basicity and Al 2O 3 Content on Modification and Removal of Inclusions in Steel 65 Mn
Liu Huijie, Wan Yong, Zhao Heming , Li Jie , Cao Ruihong
Special Steel . 2017, (4): 38 -42 .