Effect of Cu Content on Structure and Properties of Maraging Stainless Steel 0Cr17Ni4Cu4Nb
Wang Jianxing, Yang Gang, Zhang Zhongmo, Zhao Yan , Tang Guangming, Wei Xiaoming, Shen Chao, Huang He
Special Steel . 2017, (3): 66 -69 .