ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of End-Rolling Temperature and Cooling Process on Carbide Network in Φ 36 mm Bearing Steel GCr15
Deng Xiangbin, Hu Zhaofeng, Feng Jiebin, Zhang Zhengbo , Ye Dexin
Special Steel . 2017, (4): 57 -59 .