ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Analysis on Corner Cracks of Angle Steel Q420C Rolled from 180 mm x 180 mm Cast Billet and Process Improvement
Zhao Bin , Cui Huaizhou , Wang Chengyi , Wu Wei , Wang Xin