ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Evolution of Inclusions in Gear Steel 18CrNiMo7-6 during 60t LF-VD Reflning Process
Liu Jinxin, Feng Guiping, Zhang Long, Gu Wentao, Liu Yufen
Special Steel . 2016, (6): 5 -8 .