Numerical Simulation and Analysis on Hot Continuous Rolling Process of KOCKS Mill for Φ16 mm GCr15 Bearing Steel Bar
Li Xiaolong , Cheng Weiguo , Zhou Lixin , Zhou Dunshi , Zou Hui
Special Steel . 2016, (5): 5 -9 .